Aug 18, 2023 #1 ntattose Structural Apr 13, 2011 43 0 0 US Does anyone have a weight for a 13" 3 wythe brick wall?
Aug 18, 2023 #2 JAE Structural Jun 27, 2000 15,432 0 36 US Standard single wythe brick (3 5/8 in thick) is 35 psf. I typically use 40 psf for new design. For a 3-wythe wall I’d use 3 x 40 = 120 psf. Upvote 0 Downvote
Standard single wythe brick (3 5/8 in thick) is 35 psf. I typically use 40 psf for new design. For a 3-wythe wall I’d use 3 x 40 = 120 psf.
Aug 18, 2023 Thread starter #3 ntattose Structural Apr 13, 2011 43 0 0 US I use 40 psf for hollow brick veneer. These old 3 wythe walls are solid brick with 2 layers of mortar. I'm afraid this weighs more, but I'm not sure. Upvote 0 Downvote
I use 40 psf for hollow brick veneer. These old 3 wythe walls are solid brick with 2 layers of mortar. I'm afraid this weighs more, but I'm not sure.
Aug 18, 2023 #4 BAretired Structural Nov 16, 2008 10,839 0 36 CA I believe 120 psf is about right, but if you're worried, make it 150 psf, same as concrete. Surely it doesn't make a great deal of difference to your calculations. Upvote 0 Downvote
I believe 120 psf is about right, but if you're worried, make it 150 psf, same as concrete. Surely it doesn't make a great deal of difference to your calculations.
Aug 18, 2023 #5 dik Structural Apr 13, 2001 25,564 0 36 CA Isn't that what load factors are for? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik Upvote 0 Downvote
Isn't that what load factors are for? -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik
Aug 18, 2023 #6 dik Structural Apr 13, 2001 25,564 0 36 CA If it does, you may have other problems... -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik Upvote 0 Downvote
If it does, you may have other problems... -----*****----- So strange to see the singularity approaching while the entire planet is rapidly turning into a hellscape. -John Coates -Dik