30 NCD 16 Alternative Spec

Status
Not open for further replies.

ZakBarrett

Aerospace
Jun 26, 2006
1
Hello All

I am trying to find an alternative steel specification to replace the french 30NCD16 called up on a drawing. Do any of you know of any? The part to manuafactured from the material is a small collar.

Many thanks!

Zak
 
Replies continue below

Recommended for you

You have not provided nearly enough information for anyone to provide a meaningful answer. What is the size of the part? What are the requirements for final mechanical properties? What is the potential failure mode (wear, fatigue, corrosion, fracture, etc.)? Why do you need a different grade? Is it due to lack of availability in North America?
 