Hi All,
I have a 1" super duplex (ASTM A790) pipe that has had a 316 blind flange (150lb) installed. Piping spec calls for A182 Gr F55 to ASME B16.5, but for various reasons, this temporary solution was used. There has now been a request to extend this temporary solution to circa 1 year (mod made 2 weeks ago).
Additional materials:
[ul]
[li]Gaskets are SPWD 6 Mo, bolting is A276.[/li]
[li]Process medium is produced water at atmospheric pressure and ambient temperature (0 degC - 15 degC)[/li]
[/ul]
Obviously, I am concerned about the potential for galvanic corrosion but I am fairly new in my role and lack the experience to have an informed answer off the top of my head -- hoping for some insights here?
Thanks,
J.
I have a 1" super duplex (ASTM A790) pipe that has had a 316 blind flange (150lb) installed. Piping spec calls for A182 Gr F55 to ASME B16.5, but for various reasons, this temporary solution was used. There has now been a request to extend this temporary solution to circa 1 year (mod made 2 weeks ago).
Additional materials:
[ul]
[li]Gaskets are SPWD 6 Mo, bolting is A276.[/li]
[li]Process medium is produced water at atmospheric pressure and ambient temperature (0 degC - 15 degC)[/li]
[/ul]
Obviously, I am concerned about the potential for galvanic corrosion but I am fairly new in my role and lack the experience to have an informed answer off the top of my head -- hoping for some insights here?
Thanks,