Dee2e
Industrial
- Sep 15, 2022
- 4
Hello
I am experiencing a smut issue when pickling aluminium for powder-coating. The acid etching is being conducted in a steel bath (316 grade) with approx 1.6% sulphuric acid solution.
The bath is turning green over time and producing smut.
The aluminium goes through a cleaning inspection with isoproponol used to wipe off any residual machine oils prior to pickling.
What could be causing the excessive smut level, discoloration in the acid bath.
Suggestions welcome.
Thank you for the help.
I am experiencing a smut issue when pickling aluminium for powder-coating. The acid etching is being conducted in a steel bath (316 grade) with approx 1.6% sulphuric acid solution.
The bath is turning green over time and producing smut.
The aluminium goes through a cleaning inspection with isoproponol used to wipe off any residual machine oils prior to pickling.
What could be causing the excessive smut level, discoloration in the acid bath.
Suggestions welcome.
Thank you for the help.