We are supplying a lot of A356 alloy castings in T6 condition.Our machining partner complains of shrinkage and blowhole and rejects the castings on many occasions.
Whereas when we do a rough machining of these bores and conduct a Dye Penetrant test, it does not reveal any porosity.
With joint discussions and analysis, we could come to some conclusion that this occurs when the machining process engineer uses PCD(Poly Crystallind Diamond) inserts and goes for very high speed and feed this problem occurs.
We feel this could be due to pull out silicon from the bores.
The same phenomenon is not occuring on the facing sides but only when the cutting direction is perpendicular as in bore machining operations.
Would very much appreciate inputs to go into this phenomenon deeper.I will also provide cutting speed and feeds in subsequent mails.
Whereas when we do a rough machining of these bores and conduct a Dye Penetrant test, it does not reveal any porosity.
With joint discussions and analysis, we could come to some conclusion that this occurs when the machining process engineer uses PCD(Poly Crystallind Diamond) inserts and goes for very high speed and feed this problem occurs.
We feel this could be due to pull out silicon from the bores.
The same phenomenon is not occuring on the facing sides but only when the cutting direction is perpendicular as in bore machining operations.
Would very much appreciate inputs to go into this phenomenon deeper.I will also provide cutting speed and feeds in subsequent mails.