From AL.com, | 9-18-2016 | by Dennis Pillion
On the morning of Sept. 9, an inspector with the Alabama Surface Mining Commission was performing a routine monthly check of an old coal mine in Shelby County when he noticed "a strong odor of gasoline" as well as a sheen on the surface of one of the retention ponds.
The gasoline he was smelling came from Colonial Pipeline's Line 1, an underground pipeline three feet in diameter that normally pushes 1.3 million barrels of gasoline per day from refineries in Houston to distribution centers across the Southeast and along the eastern seaboard.
That 36-inch line, built in 1963, has been estimated to supply the east coast of the United States with up to 40 percent of its gasoline supply. Colonial Pipeline initiated a shutdown of Line 1 within 20 minutes of receiving the report about a potential leak.
That section of pipeline remains closed. Eight days later, official estimates climbed to 336,000 gallons of lost gasoline. More than 700 people were working around the clock to dig up the pipe, plug the leak, clean up the old mining property south of Birmingham and restore supply.
With the flow of gasoline interrupted, the governors of six states have declared a state of emergency to allow truck drivers to work longer shifts to head off shortages at the pumps.
Gasoline is now being shipped by alternate routes throughout the southeast. Alternate pipelines are being used, and gasoline is even being shipped by tanker ship from Houston to New York.
Colonial announced Saturday the company will construct a temporary pipeline to bypass the spill site in hopes of restoring gasoline flows more quickly. No timetable was given for completing the bypass line."
On the morning of Sept. 9, an inspector with the Alabama Surface Mining Commission was performing a routine monthly check of an old coal mine in Shelby County when he noticed "a strong odor of gasoline" as well as a sheen on the surface of one of the retention ponds.
The gasoline he was smelling came from Colonial Pipeline's Line 1, an underground pipeline three feet in diameter that normally pushes 1.3 million barrels of gasoline per day from refineries in Houston to distribution centers across the Southeast and along the eastern seaboard.
That 36-inch line, built in 1963, has been estimated to supply the east coast of the United States with up to 40 percent of its gasoline supply. Colonial Pipeline initiated a shutdown of Line 1 within 20 minutes of receiving the report about a potential leak.
That section of pipeline remains closed. Eight days later, official estimates climbed to 336,000 gallons of lost gasoline. More than 700 people were working around the clock to dig up the pipe, plug the leak, clean up the old mining property south of Birmingham and restore supply.
With the flow of gasoline interrupted, the governors of six states have declared a state of emergency to allow truck drivers to work longer shifts to head off shortages at the pumps.
Gasoline is now being shipped by alternate routes throughout the southeast. Alternate pipelines are being used, and gasoline is even being shipped by tanker ship from Houston to New York.
Colonial announced Saturday the company will construct a temporary pipeline to bypass the spill site in hopes of restoring gasoline flows more quickly. No timetable was given for completing the bypass line."