Hi,

I'm performing a heat treatment simulation with ansys 13.0. I need data on the specific heat of 4130 when it's at 900-1000°C. The specific heat given in the ASM (engeneering properties of steel)end at 800°C.

Does anyone know where I can find additionnal info?