Hi Guys,
We are planning to qualify an Overlay welding procedure for:
AISI 4130
Forged Block cut to 1 inch thk. plate,
75 Ksi min. YS and 95 Ksi min. TS,
C 0.3%, Cr. 0.99%, Mn 0.52% and Mo 0.17%
with following Heat Treatment done by mill: Normalizing - 900 Deg. C, 9 hours, Quenching in Water - 880 Deg. C, 9.0 hours, Tempering - 665 Deg. C, 16 hours)
Overlay welding: SMAW Process using E316L-17 Electrodes (2.4mm and 3.2mm).
Keeping a min preheat temperature of 150 Deg. C and an interpass temperature of 200 Deg. C.
Heating the test coupon to 250-300 Deg. C for 30 mins. after welding and allowing it to cool slowly in wrapped condition. No other PWHT to be performed.
Do you think this Test Coupon will qualify the mechanical Testing? Any suggestions regarding these temperatures or controlling the Heat Inputs will be much appreciated.
We are planning to qualify an Overlay welding procedure for:
AISI 4130
Forged Block cut to 1 inch thk. plate,
75 Ksi min. YS and 95 Ksi min. TS,
C 0.3%, Cr. 0.99%, Mn 0.52% and Mo 0.17%
with following Heat Treatment done by mill: Normalizing - 900 Deg. C, 9 hours, Quenching in Water - 880 Deg. C, 9.0 hours, Tempering - 665 Deg. C, 16 hours)
Overlay welding: SMAW Process using E316L-17 Electrodes (2.4mm and 3.2mm).
Keeping a min preheat temperature of 150 Deg. C and an interpass temperature of 200 Deg. C.
Heating the test coupon to 250-300 Deg. C for 30 mins. after welding and allowing it to cool slowly in wrapped condition. No other PWHT to be performed.
Do you think this Test Coupon will qualify the mechanical Testing? Any suggestions regarding these temperatures or controlling the Heat Inputs will be much appreciated.