jjimjjones
Military
We had 7/8" dia bar 4140h heat treated, 41-50 rc. the vendor could not get a consistent rc reading on the outside ,30-54. Why would this be. Also we machined some parts and got 41-54 rc readings. Why would this be? The vendor has also tried re-heat treating the bars with the same result on the o.d. when trying hardness test(varies 30-52). The ht process is vacuum / gas, not oil quench. We want to finish machine the bar stock at the blueprint rockwell call-out(41-50rc). We also want to hold the rc to with-in 5 points on the lower end, for consistant machining purposes.Could you suggest a fix to get this material in this range, preferably 42-47 rc. Why would the od be so varied?
Thanks
Jim
Thanks
Jim