Hello,

Does anyone know of a source for 48" wide 301 Full Hard sheets (60" length). I am looking for thickness of 0.040" and 0.063", but have only been able to locate 36" widths. Any help or guidance would be appreciated.
 
Replies continue below

Recommended for you

I think Somers Thin Strip in CT is limited to 36". Have you tried AK Steel Coshocton Works?
 
No. I have not contacted them directly. I appreciate your input. I'll try tomorrow. Thanks
 
And of course ATI Ludlum.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 