I am working on a bending analysis for a part made from 520.0 sand cast aluminum (T4 temper). I am having a hard time finding mechaincal strength properties for this material that will be acceptable for airworthiness certification purposes. Same for modulus of rupture curves or charts for this material.
I have not had any luck with MMPDS-01, ANC-5 or Bruhn.
Any suggestions or thoughts on where I might find data for this material is appreciated.
I have not had any luck with MMPDS-01, ANC-5 or Bruhn.