Kipmc77
Aerospace
- Jul 26, 2021
- 3
We are making a round part per the customer drawing. The drawing is old and calls for Al 6061 per AMS-QQ-A-250/11. Plate and Sheet. That spec is superseded. The new material is AMS 4025, 4026 or 4027.
The customer may allow a substitution but, before I ask, I have a few questions:
Since it is a round part (1/2 in thick by approx. 2 in dia.) We want to ask if we can use round bar stock. For example AMS-QQ-A-200/B. It has a higher yield strength than the 4027, at 52 Ksi vs 42.9 Ksi for the 4027. Starting with bar seems easier.
Does this seem like a reasonable request?
If we were to start with the plate, what would be the typical operations and machines to use to cut the plate into a circle prior to starting the lathe operations?
Thank you
The customer may allow a substitution but, before I ask, I have a few questions:
Since it is a round part (1/2 in thick by approx. 2 in dia.) We want to ask if we can use round bar stock. For example AMS-QQ-A-200/B. It has a higher yield strength than the 4027, at 52 Ksi vs 42.9 Ksi for the 4027. Starting with bar seems easier.
Does this seem like a reasonable request?
If we were to start with the plate, what would be the typical operations and machines to use to cut the plate into a circle prior to starting the lathe operations?
Thank you