Fellow Stress Engineers:

I need to perform a fatigue analysis on a component made from the above material but I do not have access to suitable SN data. 2014A-T4 extrusion is quoted on the design drawing as an alternate and has similar static strength properties. Can anyone advise as to whether it is similar to 8090 fatigue-wise? If it is not, is there another material which is fairly close to 8090 in fatigue?

Thanks in anticipation.

 
Replies continue below

Recommended for you

You need to contact Alcan Aerospace. They have fatigue data on their products.


Regards,

Cory