Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

A-301-B FB Stress Values 1

Status
Not open for further replies.

dtn6770

Mechanical
Jul 10, 2006
200
Does anyone have access to 1956 vintage API-ASME stress values for plate identified as "A-301-B FB?" Of particular interest is the allowable stress at 975 deg. F.

I'm attempting to evaluate a pressure vessel of that era and material but my employer's technical library only goes back to the 1965 edition of ASME Sec. VIII.

Thanks in advance to anyone who can help.
 
Replies continue below

Recommended for you

dtn-

From the 1956 VIII, A301-B was a 1 Cr - 1/2 Mo material with a 60 ksi UTS. Allowable tensile stress was 11 ksi at 950 deg F and 7.5 ksi at 1000 deg F. Interpolation is allowed so at 975 the allowable would be 9.25 ksi.

jt
 
Thanks jte! You slam-dunked it; the composition and tensil strength you cited are consistent with what I've found on some other documents. The 9.25 ksi allowable is exactly what I need.
 