My question is considerably simple

What is the difference between A106Gr A and A106Gr B

Thanks
 
Replies continue below

Recommended for you

basically

tensile
yield
allowable stress

small chemistry difference

i can't remember the last time I saw gr A specified
 
Do you know the exact values of tensile, yield and allowable stress for A106GrB and A106GrA
 
ntaylak

From Table A-1 of B31.3, Appendix A

ASTM A-106, Grade A
Tensile strength - 48 KSI
Yield strength - 30 KSI

ASTM A-106, Grade B
Tensile strength - 60 KSI
Yield strength - 35 KSI

Regards, John
 