Jul 23, 2002 #1 lutein Structural Joined Apr 24, 2002 Messages 136 Location US hi, Does anybody know what is the material properties for A304 Stainless Steel - The Modulus of Elasticity, Yield and Shear Strength? How does it compared to 846M1 and 846M2 ? PLease help.... Thank you in advance
hi, Does anybody know what is the material properties for A304 Stainless Steel - The Modulus of Elasticity, Yield and Shear Strength? How does it compared to 846M1 and 846M2 ? PLease help.... Thank you in advance
Jul 30, 2002 #2 Guest AISI 304 YIELD STRENGTH 2% OFFSET 38,000 psi ULTIMATE STRENGTH 90,000 psi MOD. of ELASTICITY 28.0 X 10e6 Upvote 0 Downvote
AISI 304 YIELD STRENGTH 2% OFFSET 38,000 psi ULTIMATE STRENGTH 90,000 psi MOD. of ELASTICITY 28.0 X 10e6
Aug 20, 2002 #3 imcivilized Civil/Environmental Joined Aug 19, 2002 Messages 7 Location CA I found a good website with stainless properties... http://pw1.netcom.com/~dwelding/stainless.htm This might help Upvote 0 Downvote
I found a good website with stainless properties... http://pw1.netcom.com/~dwelding/stainless.htm This might help
Aug 21, 2002 Thread starter #4 lutein Structural Joined Apr 24, 2002 Messages 136 Location US Thank you very much Upvote 0 Downvote