A304 Stainless Steel

Status
Not open for further replies.

lutein

Structural
Apr 24, 2002
136
hi,
Does anybody know what is the material properties for A304 Stainless Steel - The Modulus of Elasticity, Yield and Shear Strength? How does it compared to 846M1 and 846M2 ?

PLease help....
Thank you in advance
 
Replies continue below

Recommended for you

AISI 304
YIELD STRENGTH 2% OFFSET 38,000 psi
ULTIMATE STRENGTH 90,000 psi
MOD. of ELASTICITY 28.0 X 10e6
 