A519-4130 Tensile Strength 1

Status
Not open for further replies.

sw23cyp

Mechanical
Aug 31, 2011
27
The MTR for a piece of A519-4130 (SR) we received lists its tensile strength at 104 ksi and yield strength at 88.5 ksi. Table S2, of ASTM A519-06, lists the A519-4130 (SR) with tensile and yield as 105 ksi and 85 ksi, respectively. Is there an allowable variance in the ASTM tensile strength?
 
Replies continue below

Recommended for you

That table lists typical values to expect on testing. The MTR is actually in excellent agreement with them. They are not specified limits. Applicable limits would have to be specified by the purchaser if they have mechanical requirements for A519 material; this is the reason mechanical testing is mentioned in the spec as a supplemental requirement.
 
Thank you for your guidance, mrfailure.
 