Mous1747
Mechanical
- Apr 11, 2013
- 91
I’m my plant we have a A53 GR. B pipe that was designed for max temp of 750F as per B31.3
However this pipe was exposed to 950F for almost 10 hours
The pipe didn’t fail or anything but we are concerned that the hardness gone above the limits
Is there max hardness allowed for this pipe that we shouldn’t go above?
However this pipe was exposed to 950F for almost 10 hours
The pipe didn’t fail or anything but we are concerned that the hardness gone above the limits
Is there max hardness allowed for this pipe that we shouldn’t go above?