Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AAL Overhead Conductor

Status
Not open for further replies.

joan271273

Electrical
Sep 26, 2000
119
Can someone indicate the capacity of a 4/0 AWG AAL conductor, I cannot find AAL data.

Thanks
 
Replies continue below

Recommended for you

Suggestion: Visit
for more info on AAL usage
and Reference:
1. Table 4-22 Aluminum Conductors on page 4-64
4/0 "Oxlip"
0.1663 in**2
365 A current carrying capacity (under certain constraints, e.g. conductor temperature rise 40°C over 40°C ambient, 2ft/sec crosswind, and emissivity factor of 0.5 without sun)
7 x 0.1739 number and diameter of wires, in
0.522 conductor diameter, in
3830 rated strength, lb
198.7 nominal weight in lb per 1000'
etc.