MyNameIsUser
Mechanical
Hello,
i was wondering how abaqus interpolates the material behaviour when i enter plastic properties such as e.g.
Stress (MPa) / Strain (10^-3 in/in)
0 / 0
12.0 / 0.219
26.0 / 0.417
Lets say i run a tensile or compression test. What happens when the (true) strain is between 0.219 and 041? Is the "young's module" (does this have a name in the plastic deformation region?) of that region calculated as (26-12)/(0.417-0.219) MPa?
Thank you for any help
i was wondering how abaqus interpolates the material behaviour when i enter plastic properties such as e.g.
Stress (MPa) / Strain (10^-3 in/in)
0 / 0
12.0 / 0.219
26.0 / 0.417
Lets say i run a tensile or compression test. What happens when the (true) strain is between 0.219 and 041? Is the "young's module" (does this have a name in the plastic deformation region?) of that region calculated as (26-12)/(0.417-0.219) MPa?