Hello everyone,
I'm currently doing a finite element analysis of a composite plate (45/0/0/-45/90/-45/0/0/45) under tensile load.
I'm using 2 softwares to calculate the F.I. according Tsai Wu theory.
Patran/Nastran gives me : FI (90deg ply) = 0.65, FI (45deg ply)=0.25 and FI(0deg ply) = -0.1
SAMCEF and hand calculations gives me the same results.
However, when I run the analysis in Abaqus, I have some problems.
All the stresses (S11,S12,S22) in each ply are the same as Patran or Samcef but the Tsai Wu failure indices are different.
FI (90deg ply) = 0.65, FI (45deg ply)=0.35 and FI(0deg ply) = 0.21
I have checked the allowable stresses but it's ok. In addition to that, failure indices according the max stress theory match the results coming from Patran.
Moreover, if I perform hand calculations with the stresses given by Abaqus and the tsai wu equation given in Abaqus documentation, I get the Patran results. But Abaqus viewer plots the wrong indices...
I have heard about the fact that Abaqus does not manage the negative failure indices...
Does anyone of you could help me to overcome this problem???
Thank you
I'm currently doing a finite element analysis of a composite plate (45/0/0/-45/90/-45/0/0/45) under tensile load.
I'm using 2 softwares to calculate the F.I. according Tsai Wu theory.
Patran/Nastran gives me : FI (90deg ply) = 0.65, FI (45deg ply)=0.25 and FI(0deg ply) = -0.1
SAMCEF and hand calculations gives me the same results.
However, when I run the analysis in Abaqus, I have some problems.
All the stresses (S11,S12,S22) in each ply are the same as Patran or Samcef but the Tsai Wu failure indices are different.
FI (90deg ply) = 0.65, FI (45deg ply)=0.35 and FI(0deg ply) = 0.21
I have checked the allowable stresses but it's ok. In addition to that, failure indices according the max stress theory match the results coming from Patran.
Moreover, if I perform hand calculations with the stresses given by Abaqus and the tsai wu equation given in Abaqus documentation, I get the Patran results. But Abaqus viewer plots the wrong indices...
I have heard about the fact that Abaqus does not manage the negative failure indices...
Does anyone of you could help me to overcome this problem???
Thank you