Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Abrasive Slurry Erosion Rate Formulas 2

Status
Not open for further replies.

ianmcdz

Mechanical
Sep 19, 2009
21
Hello,

I'm looking for a formula that relates pipe material properties and service to erosion rates due to an abrasive slurry.

Thanks!
 
Replies continue below

Recommended for you

Erosive properties of a slurry depend on characteristics of both your particulate and medium. And when considering the medium, it is not only the bulk properties that are important, but corrosivity can also be important.

There are too many variables involved to give you a direct answer. Your best bet would be to perform a literature search, being as specific as possible about your system (media, piping material etc).
 
If you can contact Sala International AB Sweden,they have a lot of information available on slurry wear. Remember,the influence of several parameters will ultimately determine wear rate,there is no, one controlling factor.I used to manufacture slurry pump parts for them.

Learn the rules,so you know how to break them properly.
Dalai Lama

_____________________________________
 
i don't know exactly what you mean by slurry but there are standards to evaluate the erosion effect of a fluid in process piping.
this is for oil&gas facilities:

Erosive wear in piping systems (DNV RP O501):


Erosion in Disturbed Liquid/Particle Pipe Flow:
Effects of Flow Geometry
and Particle Surface Roughness



s