In Which part of ASME IX Ed.2019 can you find the acceptance criteria for visual inspection of welders qualification.
I need to know the acceptance criteria for refoircement, undercut, etc

Thank you for your answers...
 
Replies continue below

Recommended for you

Article I has the acceptance criteria if I remember correctly. However, Section IX is very sparse on visual criteria. There are no visual criteria for overlap, undercut, reinforcement, porosity. etc.

Best regards - Al
 