7788_011
Structural
- Feb 7, 2022
- 24
In ACI 318-11 commentary, I have found the following in regard to dowel action in shear transfer, which is removed from ACI 318-19, in addition to shear friction.
However, I am not getting why dowel action is expressed as AcK1 which has nothing to do with dowel bars? (I don't have reference 11.45 & 11.46. Can anyone please explain)?
However, I am not getting why dowel action is expressed as AcK1 which has nothing to do with dowel bars? (I don't have reference 11.45 & 11.46. Can anyone please explain)?