I have a mixture of acid gas that is (by mass) 73% CO2, 26% H2S, and about 0.2% H2O with trace hydrocarbons. The acid gas is compressed to 1100 psig and then flows to the injection well through a buried carbon steel pipeline.

My concern is that of an aqueous phase may condense one the gas hits the colder pipeline and cause localized corrosion. Should I be worried? Are there any good epoxy coatings for this type of application? I had originally planned on dehydrating the gas, but I have run into some budgetary and time constraints.
 
Replies continue below

Recommended for you

Fair enough, BALA0610, but watch out for supersturation. Make sure residense times and conditions in the cooler, and downstream, are adequate.
 