On another note, aren't there "three" types of Amines? One that works on piping systems "close" to the boiler, another that works on the piping systems "far" from the boiler, and now a third, which is a combination of the first two, hoping to work on systems that have long runs of pipe, and to also be able to coat the piping that is close to the boiler.
By coating the inside of the piping/coils, etc. it protects the piping from corrosion from such as carbonic acid, as an example.