Apr 17, 2003 #1 bwitt Automotive Apr 17, 2003 2 0 0 US Is there any low to med viscosity adhesive (other than hot melt) that will bond to untreated PP, PP based hot-melt adhesive, PC, and Acrylic?
Is there any low to med viscosity adhesive (other than hot melt) that will bond to untreated PP, PP based hot-melt adhesive, PC, and Acrylic?
May 28, 2003 #2 CalculatorDave Mechanical May 26, 2003 46 0 0 US There are some adhesive transfer tapes that are supposed to adhere well to low surface energy plastics, such as those you have mentioned. Trying looking up adhesive transfer tape #926 at 3M's web site: http://www.3m.com Upvote 0 Downvote
There are some adhesive transfer tapes that are supposed to adhere well to low surface energy plastics, such as those you have mentioned. Trying looking up adhesive transfer tape #926 at 3M's web site: http://www.3m.com
Jun 30, 2003 #3 Glueguy Materials Dec 3, 2002 34 0 0 US My first guess would be a CA (cyanoacrylate) or an acrylic transfer tape that Dave mentioned. You may try using a urethane as a low cost bond. I hope I've helped, John Schrock http://www.glubie.com Upvote 0 Downvote
My first guess would be a CA (cyanoacrylate) or an acrylic transfer tape that Dave mentioned. You may try using a urethane as a low cost bond. I hope I've helped, John Schrock http://www.glubie.com