One of our customers has quesioned the affect on the corrosion resistance and the ISO15156 compliance of Nitrocarburizing 625 weld overlay on F22. Anyone have any thoughts?
 
Replies continue below

Recommended for you

A little more information about the configuration of the components involved would help.
 
It's basicaly a cylindrical part, with a variety of IDs, inlayed over a section of the bore where seals are in contact. The whole thing is nitrocarburized. The bore is exposed to oil well production fluids.
 