Dear All,
We have some requirements for Welding connector (API 5L X-60 grade, 30" Wall thickness 1"). This connector will be welded to Conductor Pipe (API 5L X-52, 30" Wall thickness WT 1") at Drilling Rig site.
But our suppliers are offering below material specs. for Welding connector.
Supplier 1: Welding connector w/material grade AISI 4130 60 KSI (forge) w/ Carbon equivalent (CE value): 0.7-0.73.
S2: Welding connector with material grade AISI 4130 90 KSI (forge) with Carbon equivalent (CE value): 0.71-0.73
S3: Welding connector with material grade AISI 4130 100-110 KSI (forge) with CE value: 0.73-0.75
Our suppliers are claiming that all above mentioned grades are compatible and there will be no weldability issues with Conductor pipe material grade API 5L X-52.
My queries are as:
• Can we accept all above mentioned substitutional grades (yield strength: 60 ksi or 90 ksi or 100 ksi)?
• Is there any weldability issue with AISI 4130 90 ksi or 110 ksi material (high yield)?
• As per our standard, the maximum CE value is 0.43; but, suppliers proposed CE values ranges from 0.70 to 0.75. What is the
average CE value for AISI 4130 forging material?
• If we accept any of the above grades (60 or 90 110 ksi), what are the precautions to be taken w.r.t. welding at Rig site
(Welding of AISI 4130 90/110 KSI with API 5L X 52)?
Any advice is highly appreciated.
We have some requirements for Welding connector (API 5L X-60 grade, 30" Wall thickness 1"). This connector will be welded to Conductor Pipe (API 5L X-52, 30" Wall thickness WT 1") at Drilling Rig site.
But our suppliers are offering below material specs. for Welding connector.
Supplier 1: Welding connector w/material grade AISI 4130 60 KSI (forge) w/ Carbon equivalent (CE value): 0.7-0.73.
S2: Welding connector with material grade AISI 4130 90 KSI (forge) with Carbon equivalent (CE value): 0.71-0.73
S3: Welding connector with material grade AISI 4130 100-110 KSI (forge) with CE value: 0.73-0.75
Our suppliers are claiming that all above mentioned grades are compatible and there will be no weldability issues with Conductor pipe material grade API 5L X-52.
My queries are as:
• Can we accept all above mentioned substitutional grades (yield strength: 60 ksi or 90 ksi or 100 ksi)?
• Is there any weldability issue with AISI 4130 90 ksi or 110 ksi material (high yield)?
• As per our standard, the maximum CE value is 0.43; but, suppliers proposed CE values ranges from 0.70 to 0.75. What is the
average CE value for AISI 4130 forging material?
• If we accept any of the above grades (60 or 90 110 ksi), what are the precautions to be taken w.r.t. welding at Rig site
(Welding of AISI 4130 90/110 KSI with API 5L X 52)?
Any advice is highly appreciated.