AISI 4140

Status
Not open for further replies.

nrgent

Mechanical
Mar 28, 2008
3
Hi,
I would like to know the differace between 4140 to E-4140.
What the refers to?

Thx
 
Replies continue below

Recommended for you

The "E" means it is electric furnace melted rather than basic oxygen furnace melted.
 