Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations KootK on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

AL extrusion design

Status
Not open for further replies.

Kinish

Mechanical
Dec 16, 2005
12
I am designing an aluminium extrusion profile for impact bars.
A T-slot is needed for T-bolt to fasten the impact bar to its bed.
Large surface area is required for bonding of rubber to AL section.

Is there any specific data I should be aware of when designing this profile? i.e. min/max radii for dies etc.
 
Replies continue below

Recommended for you

Yes, there is specific data. Introductory information is available from the Aluminum Extruders Council:



Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Before you get too far, check that an adequate extrusion press exists. What's the diameter of the smallest circle you can draw around your extrusion profile?



Mike Halloran
Pembroke Pines, FL, USA
 
70 mm.
This should be fine as I am modifying an existing profile.
 
Status