Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

alarm 2685 Z-axis aperture overheat

Status
Not open for further replies.

minutericesentra

Industrial
Joined
Nov 7, 2019
Messages
5
Location
US
Hello, first time poster on this forum, lots of good info here.

Anyways, it's a 2006 FO-3015NT AF4000E... will a lens with a few spots cause this alarm? Or should I look for other causes?
We are cutting .062 H14 Aluminum pretty easily but can only cut for 4-5 minutes before it alarms out.

Had the same alarm with a different lens cutting .125" 304SS a few months ago, limped throught that job, now I'm stuck on this one.
 
CHeck the mirror directly above your head sounds like your issue is there
 
Well, I haven't had time to look at the mirror, but I found another lens to try and it's doing fine now... guess the old lens with spots was the culprit. I'll for sure check that mirror though next time it's down, Thanks!
 