Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IRstuff on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Allowable bend radii for .5" thick sheet metal

Status
Not open for further replies.

pbovat

Mechanical
Feb 6, 2006
11
I am trying to fabricate a 90deg bend on a .5" thick sheet metal (Gage 3/0). What are the allowable bent radii (inside) for the piece?

Is there a table?

Thanks,
-Paul
 
Replies continue below

Recommended for you

pbovat (Mechanical)
your bend rad would depend on what the material is.
I am presuming it is Aluminum.
Here are a selection of Rads taken from the Alcoa hand book
These are for .5" thick material.
2024-0 3t-5t
2024t3 6t-9t
6061t6 4t-6t
7075-0 3t-5t
7075t6 7t-12t

These are inside bends T is the thickness of the material.
B.E.
 
Hi,

could you post a link to where this Alcoa handbook can be gotten?