Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Allowable shear load SAE Grade 5 bolt

Status
Not open for further replies.

spike

Structural
Jun 7, 1999
46
Does anyone have any data on the allowable shear load for a SAE J429 Grade 4 bolt?
 
Replies continue below

Recommended for you

SAE Grade 5 medium carbon steel quenched and tempered
1/4 thru 1 inch Yield (psi)=92,000 Ultimate Tensile Strength (psi)=120,000

One method used to calculate the value is the American Institute of Steel Construction (AISC) Manual of Steel Construction, Allowable Stress Design. Using this method, the allowable tensile stress, Ft, and the allowable shear
stress, Fv, are calculated as follows:

Ft = 0.33 x Fu
Fv = 0.17 x Fu

Where Fu = minimum specified ultimate tensile
strength for the steel material.
This stress is then applied to the gross nominal area of the threaded section to calculate the load in pounds.

See spreadsheet at:

also
Mil-Handbook 5 list Fv = 0.60 x Fu
 
Status
Not open for further replies.

Part and Inventory Search