Oct 6, 2020 #1 BDBC Petroleum Oct 6, 2020 5 0 0 FR Hi everyone, Does anyone know the allowable stress as per ASMME B36.10M for A106 gr.B pipe? Thanks in advance for your help
Hi everyone, Does anyone know the allowable stress as per ASMME B36.10M for A106 gr.B pipe? Thanks in advance for your help
Oct 6, 2020 #2 XL83NL Mechanical Mar 3, 2011 3,043 0 36 NL It depends on the design code. Which code is applicable? Huub - You never get what you expect, you only get what you inspect. Upvote 0 Downvote
It depends on the design code. Which code is applicable? Huub - You never get what you expect, you only get what you inspect.
Oct 6, 2020 Thread starter #3 BDBC Petroleum Oct 6, 2020 5 0 0 FR Hi XL83NL, Thanks for your reply. Design code is ASME B31.3 Upvote 0 Downvote
Oct 6, 2020 Thread starter #4 BDBC Petroleum Oct 6, 2020 5 0 0 FR Do you by any chance also know the allowable stress for ASTM A790 & A928 pipes? Same design code ASME B31.3 Upvote 0 Downvote
Do you by any chance also know the allowable stress for ASTM A790 & A928 pipes? Same design code ASME B31.3
Oct 6, 2020 #5 TGS4 Mechanical Nov 8, 2004 3,891 0 36 CA That information is contained in ASME B31.3. You do have a copy of the Code to which you are designing, right? Upvote 0 Downvote
That information is contained in ASME B31.3. You do have a copy of the Code to which you are designing, right?