What is allowable stress for ASTM A-519 Grade 4130 tube per B31.3?
It is 15000 psi service, room temperature, Tensile ultimate strength is 105000, yield 85000.
Is it 56667 psi?
Can I use K304.1.2 eq 34a for wall thickness calculations?
It is 15000 psi service, room temperature, Tensile ultimate strength is 105000, yield 85000.
Is it 56667 psi?