I have a requirement for SB167 UNS NO6601 (alloy 601) pipe. does all 601 pipe come solution annealed? I am requiring it with a solution annealed HT process, and I am not sure if they come otherwise.

thanks
 
Replies continue below

Recommended for you

cmn8226;
I reviewed SB 167-01, and this specification provides the following options for N06601;

hot-worked annealed
cold worked annealed


annealed = solution annealed performed at 2100-2250 deg F, and either quenched in water or rapidly cooled.
 