Gentlemen,
Your thoughts would be appreciated regarding the pitting resistance of alloy 825 under the below service conditions for an gas producing inlet manifold, piping and slug catcher.
H2S: 3%mol
CO2: 5%mol
Temperature: 150 F
Pressure: 650 psig
Chloride content (of produced water): 150,000ppm
bicarbonate content (of produced water): 50ppm
Heavy sludge and halite salts are expected
As per NACE/MR0175 / ISO 15156, there are no concerns with SSC, however, I was wondering if there are any significant risk of pitting or under-deposit corrosion, given the low PREN of the alloy and that chloride content is above 150,000ppm and significant amount of deposit and (mainly halite salts) and sludge is expected.
I have seen other threads namely Link with interesting info regarding cracking risks. I haven’t found many literature references for pitting and under-deposit risk.
Thank you
Your thoughts would be appreciated regarding the pitting resistance of alloy 825 under the below service conditions for an gas producing inlet manifold, piping and slug catcher.
H2S: 3%mol
CO2: 5%mol
Temperature: 150 F
Pressure: 650 psig
Chloride content (of produced water): 150,000ppm
bicarbonate content (of produced water): 50ppm
Heavy sludge and halite salts are expected
As per NACE/MR0175 / ISO 15156, there are no concerns with SSC, however, I was wondering if there are any significant risk of pitting or under-deposit corrosion, given the low PREN of the alloy and that chloride content is above 150,000ppm and significant amount of deposit and (mainly halite salts) and sludge is expected.
I have seen other threads namely Link with interesting info regarding cracking risks. I haven’t found many literature references for pitting and under-deposit risk.