Jan 6, 2016 #1 afeefa Mechanical Jan 6, 2016 2 0 0 KW Good Day Everybody, Due to non-availability of material, required alternate material equivalent to 14" NPS A234 WP11 SCH 120 TEE. Thanks in advance. KAL
Good Day Everybody, Due to non-availability of material, required alternate material equivalent to 14" NPS A234 WP11 SCH 120 TEE. Thanks in advance. KAL
Jan 6, 2016 #2 BigInch Petroleum Jun 21, 2006 15,161 0 0 GB You might be able to find similar in a slightly higher strength, WPHY-42 Is the material a problem, or is it actually the Sch 120 thickness that you can't find. Upvote 0 Downvote
You might be able to find similar in a slightly higher strength, WPHY-42 Is the material a problem, or is it actually the Sch 120 thickness that you can't find.
Jan 6, 2016 1 #3 weldstan Materials Jun 24, 2011 2,730 0 36 US It is assumed that WP11 was specified for service conditions like high temperature or hydrogen service. In that case try WP22 or WP12. Upvote 0 Downvote
It is assumed that WP11 was specified for service conditions like high temperature or hydrogen service. In that case try WP22 or WP12.
Jan 6, 2016 #4 ricklts Mechanical Sep 15, 2010 94 0 0 US have you looked at/into/for A182-F11 or F22 forged equivalents? Upvote 0 Downvote
Jan 7, 2016 Thread starter #5 afeefa Mechanical Jan 6, 2016 2 0 0 KW Dear All, Good Day, Thanks for your comments. Service : Ultra High Pressure steam. SCH 120 A234 WP11 is found as off spec. and not available presently. Hence, planned to utilize WP12 SCH 80 on temporary basis till the proposed off spec. material arrival. Upvote 0 Downvote
Dear All, Good Day, Thanks for your comments. Service : Ultra High Pressure steam. SCH 120 A234 WP11 is found as off spec. and not available presently. Hence, planned to utilize WP12 SCH 80 on temporary basis till the proposed off spec. material arrival.
Jan 7, 2016 #6 braham0793 Mechanical Sep 3, 2015 36 0 0 PE The thickness of the fixture is to be reduced by 9 mm, it is too in my opinion not risk the line to place said accessory designer see if you can make a graft tube 14 ". Otherwise quoted by a tee in sch-160 which is more commercial. Upvote 0 Downvote
The thickness of the fixture is to be reduced by 9 mm, it is too in my opinion not risk the line to place said accessory designer see if you can make a graft tube 14 ". Otherwise quoted by a tee in sch-160 which is more commercial.