Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Aluminum 380 corrosion in a rinse tank

Status
Not open for further replies.

tallgair

Industrial
Sep 7, 2003
2
I am currently having trouble with Die cast parts of aluminum 380 corroding after being rinsed. I am currently looking at an additive called Renopas #1 but I am unsure of how effective if would be. I am looking for any information on the product as well as anyone who has used it in their operation.
 
Replies continue below

Recommended for you

Me, too, but what do you mean by rinse? Are you referring to quenching after die casting or do you mean washing? Is this a new problem?
 
Status
Not open for further replies.

Part and Inventory Search