Hello all, i am new to this metallurgy forum. I am involved in materials work.

I have a question and shall be greatly thankful if anyone rsponds.

What are the yield strength and hardness values of 7075-T61?

I googled but only found tensile strength.

Thank you all

 
Replies continue below

Recommended for you

W...

Authoritative Data... Structural allowables... For aerospace grades/forms... in-pounds units...

Metallic Materials Properties Development and Standardization (MMPDS)

Pre MMPDS => MIL-HDBK-5 METALLIC MATERIALS AND ELEMENTS FOR AEROSPACE VEHICLE STRUCTURES

Battelle Aerospace Materials handbook [ASMH: see 3207, 3208]

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 