drodrig
Mechanical
- Mar 28, 2013
- 260
Hi there,
I am looking for an aluminium alloy with a high yield strength for an end plate for a vacuum chamber (it has to take 1 bar - 14.5 psi)
The outer diameter is 2500mm (8.2 ft)
The thickness is what I am trying to determinate (between 50 and 25mm / 1 inch-0.5 inch)
What alloy would you recommend?
We have some experience with type 5754 but for thick plates the yield strength is not so attractive
thanks
I am looking for an aluminium alloy with a high yield strength for an end plate for a vacuum chamber (it has to take 1 bar - 14.5 psi)
The outer diameter is 2500mm (8.2 ft)
The thickness is what I am trying to determinate (between 50 and 25mm / 1 inch-0.5 inch)
What alloy would you recommend?
We have some experience with type 5754 but for thick plates the yield strength is not so attractive
thanks