greencircle
Mechanical
- Nov 19, 2014
- 88
Not sure if this is a welding question. But I want to see if the material combination is correct. Is it possible (recommended ?) to weld Aluminum Diecast (A360) & Aluminum Extrusion (6061 T6)?
Even tough joint looks good, we noticed severe corrosion overtime.
On the first had I want to see if these 2 alloys are OK to be welded. I will try posting this question with welding perspective under the welding forum.
Thanks,
GC
Even tough joint looks good, we noticed severe corrosion overtime.
On the first had I want to see if these 2 alloys are OK to be welded. I will try posting this question with welding perspective under the welding forum.
Thanks,
GC