I am trying to decide which Al alloy to use.

I have a cylinder approx 38mm long with very thin walls (<1mm along most of it). Aluminum with black anodize is really the only option due to weight and other factors so I need to determine if I should use 6061-T6 or 7075-T6. These are the only alloys that are allowed by the customer so I can't stray from those.

The temperature range is +71C down to -41C. At low temperature there is very little radial stress but the axial stress is fairly high (given the wall thickness) and I want to make sure that it will not break. I am worried about the brittleness of 7075-T6 when compared with 6061-T6.

Any suggestions?

Thanks,
Dan
 
Replies continue below

Recommended for you

Use fracture mechanics to decide what is the allowable flaw size and see if 7075 can be used. Can you use a different temper for the 7075? A T7-style overaging can increase toughness.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Cory,
Thanks for that. I did that and they both look OK. I guess what I am really worried about is how the fracture toughness changes (if at all) when you get down to -41C.

I can't find any reference with anything but, I am assuming, at 20C and no mention of if that changes with temperature.

Dan

 
ASM Handbook Volume 19 Fatigue and Fracture has the following data:

[tt]Alloy KIc @ 24 [&deg;]C KIc @ -196 [&deg;]C
--------- ----------- ------------
6061-T651 29.1 MPa m0.5 41.6 MPa m0.5
7075-T651 22.5 MPa m0.5 27.6 MPa m0.5[/tt]

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 