I have a customer testing thread rolling and machine screws in aluminum ingots and getting lots of variability in the results. They reported that prior tests conducted in castings (engine blocks) worked well. The material is the same.
Materials are ADC10 (no heat treatment) ADC10-T5 and AC2B-T7 (Customer is in Korea).
I suspect that testing in ingots is not valid, but can't state a definitive reason. I suspect porosity perhaps.
Can anyone state if testing the screws (for torque) in ingots is, or is not, valid and any possible reasons?
Thanks