Our company is producing a 6061 aluminum extrusion product which has a number of holes that require roller burnishing.
The process itself has been successful, but I am looking for input on service temp limits of the part after the burnishing has been completed. I ask the question because we have seen a spec from an OEM which limits temperature on a similar item to 250F. Does anyony have information on how or why this specific temp was chosen?
Details are: Hole size -.4375
Expansion - .0004-.0008
Surface finish - 16 Ra maximum
Any thoughts are appreciated.
The process itself has been successful, but I am looking for input on service temp limits of the part after the burnishing has been completed. I ask the question because we have seen a spec from an OEM which limits temperature on a similar item to 250F. Does anyony have information on how or why this specific temp was chosen?
Details are: Hole size -.4375
Expansion - .0004-.0008
Surface finish - 16 Ra maximum