Hello, I am trying to find some aluminum spring material. The shape of the spring needs to be rectangular (1 ½”L x 3/8” W x 1/16” D). I don’t know the spring constant at this point but it has to be higher than what you get from typical material machined out of stock from the hardware store.

The spring will be held at one end and the other end will be moving in an arc. I don’t know the spring constant but I know what displacement I need from the high tension position to the low tension position and that’s about 5/8”.

My question is: does anyone know where I could purchase such a material even if it was not that exact profile that I need I could machine it.
Thanks,

Jacques
 
Replies continue below

Recommended for you

If you use multiple leaves you do not want to bond them- multiple leaves work to increase deflection by reducing strain, as the leaves are allowed to slide against each other. You need lubrication between the leaves, not adhesion. If you bond them together you get the same stresses and strains as you would with a full section.
 
If the parts must be food grade compatible and recyclable, I don't see why stainless steel would not be acceptable. It would make a MUCH better spring than aluminum.

 
This sounds like an application for 'Belleville-style' stacked spring-disks... or perhaps bellows-style/stacked/welded spring disks.

These could be from punched/formed from thin aluminum high strength aluminum sheet blanks assuming a suitable corrosion protective mechanism.

Regards, Wil Taylor

o Trust - But Verify!
o We believe to be true what we prefer to be true. [Unknown]
o For those who believe, no proof is required; for those who cannot believe, no proof is possible. [variation,Stuart Chase]
o Unfortunately, in science what You 'believe' is irrelevant. ["Orion", Homebuiltairplanes.com forum]
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor