Hello.
i am the operator on an amada lc 2415 3kw laser machine. i would like some help with cutting parameters on galvanized steel in 1mm, 1.2mm, 1.5mm and 2mm.
thank you very much
 
Replies continue below

Recommended for you

as a general rule i cut galavanized with the stainless steel cutting condition for the same thickness at %60 speed
 