Or someone can help me,at setting of orbital machine ami 227.With him weld inox pipe, however welds aren't just best.I searched for literature round Internet, however I found nothing, which would help me
 
Replies continue below

Recommended for you

I've had these guidelines for some time but never implemented them. See if they are any use. I suspect that some tweaking might be required depending on material.

Hope it's useful.

Failing that, why nt get in touch with AMI - in the UK they have been helpful at providing 'ballpark' values for welding for some of the people I have dealt with.
 
 http://files.engineering.com/getfile.aspx?folder=86af63a5-e387-4c46-910a-f09e2faef387&file=Tube_welding_guidelines.pdf
Thank you for answer.I already will help self with this web link little, that you sent him to me.I am interested in him,if are you welded of what kind of inox pipe,for example fi 29x1.5 neumo,dock wiler...Some case would like to hire setting for this pipe.are can for also what kind of other pipe.How it must be set pulzer, the same in all segments,or him must what to change.Some how must to be set AT-AMP-BCK- AT-PULSE-BCK,

In what kind of relationship.How much electroda moved away needle from pipe?Uniform weld is beautiful around pipe,in the side weld isn't uniformwhich, what gas uses for root shield to pipe I use formir.

I am apologising myself, my English is worse, however we already will get along somehow.Beautiful greeting from Slovenia.Once more thank you all,that will strive to cooperate.
 